NPM-Bonding Alloys / NiCr Basis
Starbond Ni
NiCr-bonding alloy for conventional, high-fusing (low expansion) ceramics. Free of beryllium, cadmium and lead. Type 3 pursuant to DIN EN ISO 22674.
- High degree of purity
- Biocompatible and extremly corrosion resistant
Advantages for Dental Technicians:
- System-free working due to very good alloy properties
- Pleasant polishing properties and easy finishing due to low hardness of 200 HV10
- Flexibilität bei der Keramikauswahl und sicheres Verblenden
- Excellent metal-ceramic bonding, even without bonder
- Optimal conditions for laser welding
- Application flexibility and easy melting, no sparking
- An oxidation firing can be omitted
Composition:
| Ni |
60.7% |
| Cr |
24% |
| Mo |
11% |
| Fe |
1.5% |
| Si |
1.8% |
| C |
<1% |
Technical properties:
| Proof stress (Rp 0.2) |
340 - 355MPa |
| Ultimate tensile strength |
490 - 510MPa |
| Elongation |
5% |
| Elastic modulus |
200GPa |
| Vickers hardness |
200 HV 10 |
| Density |
8.2 - 8,3g/cm³ |
| Melting range |
1310 - 1410°C |
| Preheating temperature |
850 - 950°C |
| Casting temperature |
1510 - 1560°C |
| CTE (20-600°C) |
14.0 x 10⁻⁶K⁻¹ |
| Laser weldable |
Yes |
| Type (DIN EN ISO 22674) |
3 |